Drawing

A drawing is the 2D document that fixes a sheet metal part's geometry, material and acceptance rules for every shop step.

Every Drawing article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A drawing is the 2D document that fixes a sheet metal part’s geometry, material and acceptance rules for every shop step. In sheet work it also records choices no other document holds. Among them are the tolerance column of the sheet, the class of a laser cut and the quality level of a weld. The standards behind those choices apply only when the drawing or the delivery documents cite them. A requirement left off the drawing is settled by the shop’s own default.

Standard Reference

ISO 9013 applies only when a drawing or a delivery document refers to it. A bare “ISO 9013” chooses no range and no class. Its 2017 text is a technical revision of the 2002 edition, so the year belongs in the reference. ISO 5817 asks for the weld quality level to be set before production, preferably at enquiry or order. Its 2023 edition changed the row on multiple imperfections. Two drawings that cite different editions may therefore describe different inspections. EN 10131 is named with its year for the same reason.
Read More

Material Line

The material line closes questions that datasheets leave open. Writing 316L rather than “stainless” fixes carbon at 0.03 % maximum, where plain 316 allows 0.08 %. A line reading only 5052 H32 leaves the yield minimum open. ASTM B209M sets it at 160 MPa (23 ksi), and BS EN 485-2 at 130 MPa (19 ksi). Cold rolled steel needs its standard, strength class, normal or special column and width class. Galvanized sheet needs the coating type, designation, standard and test basis. Where a joint depends on stacked thickness, the line says whether the nominal is bare or coated.

Cut Edge Callout

An ISO 9013 designation lists the squareness range, the roughness range and the dimensional class in a fixed order. In ISO 9013-312, squareness is in range 3, roughness in range 1 and size in class 2. A zero stands in for any value left unset. On aluminum the roughness range is better left out, since Annex A says Rz5 cannot be evaluated there. Under 2 mm (0.079 in) the squareness method has to be agreed, because the standard gives none. Mating features take the tighter class, and fit-critical features are dimensioned to each other within one cut.

Bend Callout

The inside radius is written as a number, because the punch and die opening produce a fixed radius. The Fabricator quotes a supplier’s suggestion of 1.5 t for 3.2 mm (0.125 in) 5052-H32. That is 4.8 mm (0.19 in), and a sharp corner on that sheet is outside the table. Durma’s multiples put a 2 mm (0.079 in) stainless bend in a die of 20 to 24 mm (0.79 to 0.94 in). That die forms a radius of 4.0 to 5.3 mm (0.16 to 0.21 in). A drawn radius of 2 mm (0.079 in) on that part therefore disagrees with the tooling. Writing the radius as an acceptable range removes the dispute.

Weld and Finish Notes

ISO 5817 sets no limit for spatter or temper colors at any quality level. Their acceptance therefore becomes a drawing note. A 316L part that has to resist chlorides carries its tint rule and cleaning step on the drawing. An aluminum seam takes its level from an aluminum weld standard, because ISO 5817 does not cover the metal. A finished face needs the face named, a roughness criterion and a reference sample. For powder coating, a RAL number fixes the shade on paper. Mating features are either masked or drawn with the film thickness allowed for.

Galvanized Parts

Galvanized sheet adds three lines that plain steel does not need. The first names the coating designation and its standard, such as Z275 to ASTM A653M. The second states the test basis, since a blank cut from a wide sheet carries only the single spot guarantee. The third sets the spatter and zinc burn accepted beside a seam. G30 and 30G are different products, so the standard is always named.

Design Freeze

A progressive die takes the drawing as fixed. A progressive die is designed, built and tried out before its first part, and the weeks are the toolmaker’s own figure. A change after that point becomes die rework, while laser and brake work follow an edited file. A nest check before the drawing is frozen can drop a row of blanks and save a sheet on every repeat. The drawing that leaves the first batch, with its tolerances confirmed on real parts, is the one later runs repeat.

Sheet Metal Inspection From First Article to Batch Release

Measure the first part against every requirement, then release each lot on a defined sample, with weld, coating and hardware checks tied to their standards.

First Article Inspection for Sheet Metal PartsA first article inspection measures the first part made by the production process against every requirement on the drawing and records the result. In aerospace the practice has its own standard, SAE AS9102, whose scope is to establish the baseline requirements for performing and documenting a first article inspection.

Inserting Self-Clinching Fasteners in Sheet Metal Step by Step

Cut the hole to size without deburring, check the sheet is soft enough, finish the panel, then squeeze the nut in parallel until its head meets the sheet.

How a Self-Clinching Nut Locks Into Thin SheetInstallation takes three moves. First a hole of the specified size is punched or drilled, the nut's shank is placed in it, and a press squeezes nut and sheet between parallel surfaces until the head meets the sheet.

Minimum Bend Radius by Sheet Material and Thickness

Take the minimum bend radius from the maker's table for the exact grade, temper, thickness and bend direction, then draw the radius the die forms.

Minimum Inside Bend Radius Values for Steel SheetSteel makers print the minimum as a multiple of thickness, t, and the multiple rises with strength and with thickness. The two hot-rolled cold-forming ranges below are the clearest published sets; mild cold-rolled steels such as DC01 come with formability figures but, in the makers' datasheets cited here, no printed radius.

Bend Angle and Flange Length Tolerance on Press Brake Parts

Set the bend angle tolerance from the position the flange tip has to reach, and control sheet thickness, die width and the flat pattern behind it.

Bend Angle and Flange Length Tolerance ValuesThere is no single tolerance for bent sheet metal. Durmapress says so plainly and offers planning ranges per operation instead, warning that they are a guide only and move with the material, thickness, size of part, machine, state of the tooling, number of operations and the way parts are inspected.

ISO 2768 and DIN 6930 General Tolerances for Bent Sheet Metal Parts

ISO 2768-1 covers sheet metal parts by size class; on a bent part its angular row decides fit, and DIN 6930-2 is written for stamped steel parts only.

What ISO 2768-1 Covers on a Sheet Metal DrawingISO 2768-1, first edition 1989-11-15, sets general tolerances for linear and angular dimensions without individual tolerance indications, in four classes. Its scope names sheet metal directly: it applies to the dimensions of parts produced by metal removal or parts formed from sheet metal.

ISO 1461 Hot-Dip Galvanizing of Fabricated Steel Parts

ISO 1461 sets zinc thickness by steel thickness, measures it away from edges, and expects cut edges ground and parts bent before galvanizing.

What ISO 1461 Covers for Cut and Bent Steel PartsISO 1461:2022, the fourth edition, sets out the properties and test methods of zinc coatings formed when finished iron and steel articles, some castings included, are dipped in molten zinc holding at most 2 % of other metals. Its key word is fabricated: the parts are cut, formed and welded first and galvanized afterward in batches, by a company the standard now defines as the galvanizer.

High-Strength Steel Sheet S355 and S420 and the Springback It Brings

Order S355 or S420 for bent parts as the EN 10149-2 MC grade, bend at the recommended radius, and expect more springback than mild steel.

S355 and S420 Sheet Grades in EN 10149-2 and EN 10025-2High-strength sheet for cut and bent parts comes mainly from two European product standards. EN 10025-2 covers non-alloy structural steels, the S235, S275 and S355 families with the JR, J0 and J2 suffixes that set the impact-test temperature.

Cold Rolled DC01 and Hot Rolled S235 Steel Sheet for Cut and Bent Parts

Choose DC01 for thin formed parts that need tight thickness, flatness and a clean surface, and S235 for thicker load-bearing parts, then name the standard on the order.

DC01 and S235 Compared for Laser Cut and Bent Sheet PartsDC01 is a cold-rolled non-alloy mild steel for cold forming under EN 10130, material number 1.0330, which ArcelorMittal describes as having a guaranteed maximum yield and tensile strength, a guaranteed minimum elongation and good formability. S235 is a hot-rolled carbon-manganese structural steel under EN 10025-2, described by the same mill as having a guaranteed minimum yield and tensile strength and satisfactory ductility, in JR, J0 and J2 versions that differ in impact-test temperature.

Progressive Die Stamping After Laser Cut and Bent Sheet Metal Parts

A progressive die makes parts in minutes but takes months to build and wants a design that has stopped, so quantity and design stability choose between die and laser.

What Changes When a Part Moves From Laser and Brake to a DieIn laser and brake work, a flat blank is cut by a beam from a program and bent on a press brake with standard tooling, so a part exists the day the drawing and the sheet exist. In progressive stamping, a continuous strip passes through one die set with several stations.

Powder Coated Sheet Metal Batch From Pretreatment to Cure and Inspection

A powder coating cures in minutes but depends on pretreatment, rack mass and film allowance, and a lot is judged on gloss, film and adhesion, not corrosion hours.

The Stages a Coated Batch Passes ThroughA batch of sheet metal parts goes through six stages on its way from the bare part to a coated one: pretreatment, drying, masking and hanging, application, cure, and cooling and packing. Each stage has a condition the powder maker states, and each has its own place in the schedule.

Press Brake Bending of Sheet Metal From Die Opening to Final Angle

A press brake bend is decided by the die opening, which sets radius, flange length, springback and the flat pattern, so the first piece carries every assumption of the lot.

How a Press Brake Forms a Bend in AirMost sheet metal is bent by air forming. The punch pushes the sheet into a V-shaped die, and the sheet touches only three points: the two shoulders of the die and the tip of the punch.

Laser Cut Part Dimensional Tolerance Under ISO 9013 Class 1 and Class 2

Pick the tighter or looser dimensional class per feature, read inside and outside sizes at their extremes, and anchor fit features to each other.

What Dimensional Tolerance Class 1 and Class 2 Cover on a Laser Cut PartISO 9013:2017 applies to laser cuts from 0.5 mm to 32 mm in thickness. Its clause 8 gives limit deviations for nominal dimensions in two classes, listed in Table 6 for class 1 and Table 7 for class 2.

Cold Rolled Steel Sheet Thickness Tolerance Under EN 10131

Choose the tolerance column by what the part does with a thickness error, and write the strength class and column on the order.

What EN 10131 Allows on the Thickness of a Cold Rolled SheetEN 10131 covers cold rolled flat products of uncoated and electrolytically coated steel, and ArcelorMittal's tolerance tables reproduce its thickness limits as guarantees. The tables run from 0.35 mm to 3.00 mm and apply per nominal thickness band, per width class and per yield strength class.

ISO 9013 Laser Cut Edge Quality Ranges for Squareness and Roughness

Pick a squareness range and a roughness range by thickness, add the dimensional class, and agree how thin sheet is measured.

What the ISO 9013 Ranges Tell You About a Laser Cut EdgeISO 9013:2017 presents geometrical product specifications and quality tolerances for thermal cuts in materials suitable for oxyfuel flame cutting, plasma cutting and laser cutting. Its scope runs from 3 mm to 300 mm for flame cuts, 0.5 mm to 150 mm for plasma cuts and 0.5 mm to 32 mm for laser cuts.

ISO 5817 Weld Quality Levels B, C and D for Sheet Metal Parts

Name a quality level per joint, cite the current edition, and agree how thin-sheet welds are inspected and finished.

What Quality Levels B, C and D Mean for a Sheet Metal WeldISO 5817 specifies quality levels for imperfections in fusion-welded joints in steel, nickel, titanium and their alloys. It applies to material 0.5 mm thick and above and covers fully penetrated butt welds and all fillet welds.

Galvanized Steel Sheet Coating Weight Designations for Cut and Welded Parts

Read the coating designation as a minimum zinc mass over both faces, name the standard and test basis, and plan ventilation for cutting and welding.

What a Coating Weight Designation Says About the SheetA designation states the minimum mass of zinc, or zinc alloy, on the sheet and the units it is stated in. G90 means hot-dip galvanized, with a triple spot test average of at least 0.90 ounce per square foot, counted over both sides together.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

316L Stainless Steel Sheet for Laser Cutting and Bending

Choose the molybdenum-bearing low-carbon grade for chloride exposure, plan overbend on the brake, and write the finish and weld tint rules on the drawing.

What 316L Sheet Adds Over 304L in a Cut and Bent PartType 316L is Type 316 with the carbon ceiling lowered from 0.08 % to 0.03 % by weight. Both carry 16.0 to 18.0 % chromium, 10.0 to 14.0 % nickel and 2.00 to 3.00 % molybdenum, according to the Cleveland-Cliffs product bulletin for the two types.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote