Hole

A hole in a sheet part is an internal contour, cut by laser after a pierce or punched in a die.

Every Hole article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A hole in a sheet part is an internal contour, cut by laser after a pierce or punched in a die. Its size and position shift with each later step. The laser sets it, the brake can stretch it, the weld can move it and the coating can shrink it. Each of those steps has a published rule.

Pierce and Cycle

Every internal contour starts with a pierce, a step with its own power, frequency, nozzle height and gas. On thick plate a pierce takes seconds, not fractions of one. GWEIKE prints a three-stage pierce for 22 mm (0.87 in) carbon steel on 3 kW with oxygen. Its stages run 200 ms, 2,500 ms and 3,000 ms. A nest with hundreds of small holes in 16 mm (0.63 in) plate is therefore slower than its contour length suggests. A sound program starts each cut in scrap and joins the contour with a lead-in.
Read More

Size Reading

ISO 9013 reads an inside dimension at its smallest actual size. The diameter of a cut hole is therefore the smallest one measured on the clean face. Dimensions are measured on the clean cut surface, away from dross. A mounting hole pattern at 200 mm (7.9 in) pitch may take class 2. A bolt clearance of 1 mm (0.04 in) absorbs that class.

Near a Bend

A hole placed too close to a bend line stretches into an oval. Bystronic’s rule of thumb keeps holes at least six thicknesses from the bend line. On 5052 parts, a distorted hole is the first visible sign of a bend that was too tight. A hole that must stay round near a flange is therefore moved, or cut after bending.

Die Rules

A progressive die adds rules the laser does not need. A die-pierced hole has to be large enough to punch, and holes used as pilots large enough to locate the strip. It recommends 1.2 to 1.5 times for longer tool life, since small holes risk punch breakage. Features need at least 2.0 thicknesses between them. A 2 mm (0.079 in) hole in 3 mm (0.12 in) sheet is 0.67 times the thickness. It needs a redesign before a die.

Coating Allowance

Powder film lines the whole circle of a hole. IGP’s film is 60 to 80 µm (0.0024 to 0.0031 in). A 5 mm (0.20 in) hole therefore loses 0.12 to 0.16 mm (0.005 to 0.006 in) in diameter. That figure is arithmetic from the film range, not an allowance a maker states. Threaded holes are masked, or drawn to a size that allows for the film.

After Welding

A hole that fit before welding can move. Weld shrinkage pulls the panel, so hole positions are checked after the weld. A welded assembly is checked from size to squareness to flatness and hole position. Fit-critical holes are dimensioned to each other within one cut.

Small Contours

ISO 9013 Annex A says its classes cannot be reached at small radii or sharp angles. Small holes are such contours, so their size and edge sit outside the table. Inside corners and small holes are also where heat builds and oxygen cuts burn out. A hole that matters is therefore toleranced on its own and checked on the first piece.

Sheet Metal Inspection From First Article to Batch Release

Measure the first part against every requirement, then release each lot on a defined sample, with weld, coating and hardware checks tied to their standards.

First Article Inspection for Sheet Metal PartsA first article inspection measures the first part made by the production process against every requirement on the drawing and records the result. In aerospace the practice has its own standard, SAE AS9102, whose scope is to establish the baseline requirements for performing and documenting a first article inspection.

Inserting Self-Clinching Fasteners in Sheet Metal Step by Step

Cut the hole to size without deburring, check the sheet is soft enough, finish the panel, then squeeze the nut in parallel until its head meets the sheet.

How a Self-Clinching Nut Locks Into Thin SheetInstallation takes three moves. First a hole of the specified size is punched or drilled, the nut's shank is placed in it, and a press squeezes nut and sheet between parallel surfaces until the head meets the sheet.

Bend Angle and Flange Length Tolerance on Press Brake Parts

Set the bend angle tolerance from the position the flange tip has to reach, and control sheet thickness, die width and the flat pattern behind it.

Bend Angle and Flange Length Tolerance ValuesThere is no single tolerance for bent sheet metal. Durmapress says so plainly and offers planning ranges per operation instead, warning that they are a guide only and move with the material, thickness, size of part, machine, state of the tooling, number of operations and the way parts are inspected.

ISO 2768 and DIN 6930 General Tolerances for Bent Sheet Metal Parts

ISO 2768-1 covers sheet metal parts by size class; on a bent part its angular row decides fit, and DIN 6930-2 is written for stamped steel parts only.

What ISO 2768-1 Covers on a Sheet Metal DrawingISO 2768-1, first edition 1989-11-15, sets general tolerances for linear and angular dimensions without individual tolerance indications, in four classes. Its scope names sheet metal directly: it applies to the dimensions of parts produced by metal removal or parts formed from sheet metal.

Progressive Die Stamping After Laser Cut and Bent Sheet Metal Parts

A progressive die makes parts in minutes but takes months to build and wants a design that has stopped, so quantity and design stability choose between die and laser.

What Changes When a Part Moves From Laser and Brake to a DieIn laser and brake work, a flat blank is cut by a beam from a program and bent on a press brake with standard tooling, so a part exists the day the drawing and the sheet exist. In progressive stamping, a continuous strip passes through one die set with several stations.

Powder Coated Sheet Metal Batch From Pretreatment to Cure and Inspection

A powder coating cures in minutes but depends on pretreatment, rack mass and film allowance, and a lot is judged on gloss, film and adhesion, not corrosion hours.

The Stages a Coated Batch Passes ThroughA batch of sheet metal parts goes through six stages on its way from the bare part to a coated one: pretreatment, drying, masking and hanging, application, cure, and cooling and packing. Each stage has a condition the powder maker states, and each has its own place in the schedule.

Press Brake Bending of Sheet Metal From Die Opening to Final Angle

A press brake bend is decided by the die opening, which sets radius, flange length, springback and the flat pattern, so the first piece carries every assumption of the lot.

How a Press Brake Forms a Bend in AirMost sheet metal is bent by air forming. The punch pushes the sheet into a V-shaped die, and the sheet touches only three points: the two shoulders of the die and the tip of the punch.

Laser Cutting Sheet Metal With Oxygen, Nitrogen or Air Assist Gas

Oxygen, nitrogen and air each leave a different edge on laser cut sheet, and the choice of gas settles speed, finishing work and what the next process accepts.

Which Assist Gas Cuts Which Sheet MetalThree gases cover almost all sheet work: oxygen, nitrogen and compressed air. Oxygen belongs to carbon and low-alloy steel, nitrogen to stainless steel and aluminum, and air sits between them as the cheaper trade for thin parts that tolerate a slightly darker edge.

Laser Cut Part Dimensional Tolerance Under ISO 9013 Class 1 and Class 2

Pick the tighter or looser dimensional class per feature, read inside and outside sizes at their extremes, and anchor fit features to each other.

What Dimensional Tolerance Class 1 and Class 2 Cover on a Laser Cut PartISO 9013:2017 applies to laser cuts from 0.5 mm to 32 mm in thickness. Its clause 8 gives limit deviations for nominal dimensions in two classes, listed in Table 6 for class 1 and Table 7 for class 2.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote