Laser Cutting

Laser cutting separates sheet with a focused beam while an assist gas clears the melt from the kerf.

Every Laser Cutting article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Laser cutting separates sheet with a focused beam while an assist gas clears the melt from the kerf. It is the usual first step for low quantities of sheet parts, because it needs a program and no tool. ISO 9013 covers laser cuts from 0.5 to 32 mm (0.02 to 1.26 in). Annex A of that standard lists class 1 as the typical dimensional result up to 32 mm (1.26 in).

Cutting Modes

Annex B of ISO 9013 names three kinds of laser cutting. In laser oxyfuel cutting, the beam heats the steel while an oxygen jet burns it. Fusion cutting melts the material and blows the melt out with a gas jet. Sublimation cutting evaporates the material in the cut. TRUMPF calls the oxygen mode flame cutting and the nitrogen or argon mode fusion cutting.
Read More

Beam and Kerf

TRUMPF states that the focal spot is often under 0.5 mm (0.02 in). The kerf is barely wider than the focused beam. The program therefore offsets the cut path by half the kerf, which matters most on tight mating cutouts. Annex B adds that the achievable quality differs between CO₂ and solid state sources.

Time per Sheet

Beam time is contour length over cutting speed, plus pierces and moves. A sheet of 130 blanks of 180 by 110 mm (7.1 by 4.3 in) carries 75.4 m (247 ft) of cut. At GWEIKE’s 25 to 30 m/min (985 to 1,180 in/min) for 2 mm (0.079 in) stainless on 6 kW, that is 2.5 to 3.0 minutes. A sheet is therefore a matter of minutes at the laser. The days of a lead time lie in material, bending, welding, finishing and inspection.

Machine Limits

TRUMPF lists working ranges from 3,000 by 1,500 mm (118 by 59 in) to 8,000 by 2,500 mm (315 by 98 in). The thickest cut rises with power: 25 mm (0.98 in) mild steel at 6 kW, 40 mm (1.57 in) at 24 kW. Near the top of the range, power sets the pace. GWEIKE puts 20 mm (0.79 in) stainless at 0.2 to 0.35 m/min (8 to 14 in/min) on 6 kW. On 12 kW the same plate runs at 1.2 to 1.4 m/min (47 to 55 in/min).

Effect on Later Steps

The laser edge travels into every later step. SSAB asks that thermal cut edges be deburred before bending. A laser-cut blank also has a slightly different edge from a punched one. A part moved from the laser to a progressive die is therefore checked as a new first article. Laser and brake work can follow a design that still moves, which a die cannot.

Minimum Bend Radius by Sheet Material and Thickness

Take the minimum bend radius from the maker's table for the exact grade, temper, thickness and bend direction, then draw the radius the die forms.

Minimum Inside Bend Radius Values for Steel SheetSteel makers print the minimum as a multiple of thickness, t, and the multiple rises with strength and with thickness. The two hot-rolled cold-forming ranges below are the clearest published sets; mild cold-rolled steels such as DC01 come with formability figures but, in the makers' datasheets cited here, no printed radius.

ISO 2768 and DIN 6930 General Tolerances for Bent Sheet Metal Parts

ISO 2768-1 covers sheet metal parts by size class; on a bent part its angular row decides fit, and DIN 6930-2 is written for stamped steel parts only.

What ISO 2768-1 Covers on a Sheet Metal DrawingISO 2768-1, first edition 1989-11-15, sets general tolerances for linear and angular dimensions without individual tolerance indications, in four classes. Its scope names sheet metal directly: it applies to the dimensions of parts produced by metal removal or parts formed from sheet metal.

ISO 1461 Hot-Dip Galvanizing of Fabricated Steel Parts

ISO 1461 sets zinc thickness by steel thickness, measures it away from edges, and expects cut edges ground and parts bent before galvanizing.

What ISO 1461 Covers for Cut and Bent Steel PartsISO 1461:2022, the fourth edition, sets out the properties and test methods of zinc coatings formed when finished iron and steel articles, some castings included, are dipped in molten zinc holding at most 2 % of other metals. Its key word is fabricated: the parts are cut, formed and welded first and galvanized afterward in batches, by a company the standard now defines as the galvanizer.

High-Strength Steel Sheet S355 and S420 and the Springback It Brings

Order S355 or S420 for bent parts as the EN 10149-2 MC grade, bend at the recommended radius, and expect more springback than mild steel.

S355 and S420 Sheet Grades in EN 10149-2 and EN 10025-2High-strength sheet for cut and bent parts comes mainly from two European product standards. EN 10025-2 covers non-alloy structural steels, the S235, S275 and S355 families with the JR, J0 and J2 suffixes that set the impact-test temperature.

Cold Rolled DC01 and Hot Rolled S235 Steel Sheet for Cut and Bent Parts

Choose DC01 for thin formed parts that need tight thickness, flatness and a clean surface, and S235 for thicker load-bearing parts, then name the standard on the order.

DC01 and S235 Compared for Laser Cut and Bent Sheet PartsDC01 is a cold-rolled non-alloy mild steel for cold forming under EN 10130, material number 1.0330, which ArcelorMittal describes as having a guaranteed maximum yield and tensile strength, a guaranteed minimum elongation and good formability. S235 is a hot-rolled carbon-manganese structural steel under EN 10025-2, described by the same mill as having a guaranteed minimum yield and tensile strength and satisfactory ductility, in JR, J0 and J2 versions that differ in impact-test temperature.

Progressive Die Stamping After Laser Cut and Bent Sheet Metal Parts

A progressive die makes parts in minutes but takes months to build and wants a design that has stopped, so quantity and design stability choose between die and laser.

What Changes When a Part Moves From Laser and Brake to a DieIn laser and brake work, a flat blank is cut by a beam from a program and bent on a press brake with standard tooling, so a part exists the day the drawing and the sheet exist. In progressive stamping, a continuous strip passes through one die set with several stations.

Press Brake Bending of Sheet Metal From Die Opening to Final Angle

A press brake bend is decided by the die opening, which sets radius, flange length, springback and the flat pattern, so the first piece carries every assumption of the lot.

How a Press Brake Forms a Bend in AirMost sheet metal is bent by air forming. The punch pushes the sheet into a V-shaped die, and the sheet touches only three points: the two shoulders of the die and the tip of the punch.

Laser Cutting Sheet Metal With Oxygen, Nitrogen or Air Assist Gas

Oxygen, nitrogen and air each leave a different edge on laser cut sheet, and the choice of gas settles speed, finishing work and what the next process accepts.

Which Assist Gas Cuts Which Sheet MetalThree gases cover almost all sheet work: oxygen, nitrogen and compressed air. Oxygen belongs to carbon and low-alloy steel, nitrogen to stainless steel and aluminum, and air sits between them as the cheaper trade for thin parts that tolerate a slightly darker edge.

Laser Cut Part Dimensional Tolerance Under ISO 9013 Class 1 and Class 2

Pick the tighter or looser dimensional class per feature, read inside and outside sizes at their extremes, and anchor fit features to each other.

What Dimensional Tolerance Class 1 and Class 2 Cover on a Laser Cut PartISO 9013:2017 applies to laser cuts from 0.5 mm to 32 mm in thickness. Its clause 8 gives limit deviations for nominal dimensions in two classes, listed in Table 6 for class 1 and Table 7 for class 2.

ISO 9013 Laser Cut Edge Quality Ranges for Squareness and Roughness

Pick a squareness range and a roughness range by thickness, add the dimensional class, and agree how thin sheet is measured.

What the ISO 9013 Ranges Tell You About a Laser Cut EdgeISO 9013:2017 presents geometrical product specifications and quality tolerances for thermal cuts in materials suitable for oxyfuel flame cutting, plasma cutting and laser cutting. Its scope runs from 3 mm to 300 mm for flame cuts, 0.5 mm to 150 mm for plasma cuts and 0.5 mm to 32 mm for laser cuts.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote