Meaning
EN 10051 is the European standard for the tolerances of continuously hot rolled strip, sheet and plate, grading thickness bands by yield category and width. It covers hot rolled grades such as S235 under EN 10025-2 and the cold-forming MC grades under EN 10149-2. Its bands are wider than those of EN 10131 for cold rolled sheet.Categories
ArcelorMittal’s tables list category A for yield up to 300 MPa (44 ksi), B to 360 MPa, C to 420 MPa and D to 960 MPa, with tolerances agreed separately above that. For category A at widths up to 1,200 mm (47 in), the thickness tolerance is ±0.17 mm (±0.0067 in) at 2 mm and under and ±0.20 mm (±0.0079 in) from 2.5 to 3 mm. Hot rolled forming steels under EN 10111 roll to a closer band, ±0.13 mm at 2 mm and under.Read More
Flatness
Normal flatness for categories A to C at widths up to 1,200 mm is 18 mm (0.71 in) per meter at 2 mm and under and 15 mm (0.59 in) at 2.5 to 3 mm; the special class narrows the latter to 11 mm (0.43 in). The flatness tolerances apply to sheet and plate, not to coil.Fractions
Mills sell tighter versions as fractions of the standard band. ArcelorMittal offers three quarters, one half and one third of EN 10051 on its laser-cutting coils, and SSAB delivers Domex to two thirds by default and down to one third by agreement. For a hot rolled part that is laser cut and bent, the fraction on the order is what narrows the angle scatter at the brake.