Ultimate Tensile Strength

Ultimate tensile strength is the peak strength a datasheet prints beside yield strength, and an input to press brake force estimates.

Every Ultimate Tensile Strength article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Ultimate tensile strength is the peak strength a datasheet prints beside yield strength, and an input to press brake force estimates. It enters press brake force estimates. It also shows how a grade weakens with heat. Like yield, it may be printed as a typical value or as a minimum.

Stainless Values

Cleveland-Cliffs prints typical values for 304 and 316 sheet. For 304 and 304L it gives 655 MPa (95 ksi), and for 316 and 316L 627 MPa (91 ksi). These are typical figures, so a certificate is read against ASTM A240 instead. At 538 °C (1,000 °F), 316L falls to 483 MPa (70 ksi), 77 % of its room value. At 649 °C (1,200 °F) it is 393 MPa (57 ksi).
Read More

Aluminum Values

For 5052 H32, The Fabricator’s bending column works with 228 MPa (33,000 psi), a value it takes from a materials database. Smiths lists 210 MPa (30 ksi) with no stated basis, below the B209M minimum. Full-hard H38 carries 270 MPa (39 ksi) minimum, and soft O 170 to 215 MPa (25 to 31 ksi).

In Bending Force

Durma’s force estimate multiplies bend length, thickness squared and tensile strength by 1.42, over the V opening. Take mild steel of 450 N/mm² (65 ksi), bent 1,000 mm (39 in) long at 2 mm (0.079 in) thick. Over a 16 mm (0.63 in) die, the estimate is about 160 kN (36,000 lbf). By Wila’s account, tensile strength also limits the smallest radius a sheet can form.

Substitutes

5251 is sometimes offered for 5052, and the Aluminum Association’s register shows it with less magnesium. Its listed H32 tensile minimum, 200 MPa (29 ksi), sits below that of 5052 H32.

High-Strength Steel Sheet S355 and S420 and the Springback It Brings

Order S355 or S420 for bent parts as the EN 10149-2 MC grade, bend at the recommended radius, and expect more springback than mild steel.

S355 and S420 Sheet Grades in EN 10149-2 and EN 10025-2High-strength sheet for cut and bent parts comes mainly from two European product standards. EN 10025-2 covers non-alloy structural steels, the S235, S275 and S355 families with the JR, J0 and J2 suffixes that set the impact-test temperature.

Cold Rolled DC01 and Hot Rolled S235 Steel Sheet for Cut and Bent Parts

Choose DC01 for thin formed parts that need tight thickness, flatness and a clean surface, and S235 for thicker load-bearing parts, then name the standard on the order.

DC01 and S235 Compared for Laser Cut and Bent Sheet PartsDC01 is a cold-rolled non-alloy mild steel for cold forming under EN 10130, material number 1.0330, which ArcelorMittal describes as having a guaranteed maximum yield and tensile strength, a guaranteed minimum elongation and good formability. S235 is a hot-rolled carbon-manganese structural steel under EN 10025-2, described by the same mill as having a guaranteed minimum yield and tensile strength and satisfactory ductility, in JR, J0 and J2 versions that differ in impact-test temperature.

316L Stainless Steel Sheet for Laser Cutting and Bending

Choose the molybdenum-bearing low-carbon grade for chloride exposure, plan overbend on the brake, and write the finish and weld tint rules on the drawing.

What 316L Sheet Adds Over 304L in a Cut and Bent PartType 316L is Type 316 with the carbon ceiling lowered from 0.08 % to 0.03 % by weight. Both carry 16.0 to 18.0 % chromium, 10.0 to 14.0 % nickel and 2.00 to 3.00 % molybdenum, according to the Cleveland-Cliffs product bulletin for the two types.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote