Cut Edge

A cut edge is the face a laser, flame or plasma cut leaves on a sheet part, judged by squareness, roughness, color and lower-side residue.

Every Cut Edge article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A cut edge is the face a laser, flame or plasma cut leaves on a sheet part, judged by squareness, roughness, color and lower-side residue. ISO 9013 grades the face with two values, squareness u and roughness Rz5. The gas, the speed and the sheet decide what the face looks like. The next step, whether bending, welding or coating, decides how much that matters.

Edge Values

Squareness u is the gap between two parallel lines that enclose the face profile. It includes flatness of the face, so a bow and a lean both use up the allowance. Rz5 is the mean of five consecutive peak-to-valley profile elements. Because it is peak-to-valley, it runs larger than the Ra most drawings quote. A face designation such as 2B on stainless says nothing about the cut edge. The edge therefore needs its own callout, separate from the finish of the face.
Read More

Gas Signature

Oxygen burns carbon steel and leaves a scaled, oxide-coated edge. Nitrogen only blows the melt out, so stainless and aluminum keep a bright edge. Air sits between the two and leaves a darker edge on stainless and more dross on aluminum. Trumpf describes drag lines that bend away from the beam as speed rises. A wrong cutting speed raises roughness and leaves burr on the lower edge.

Size Reading

ISO 9013 reads part size on the clean surface of the cut, not on a surface covered with dross. Outside dimensions are read at their largest actual size. Inside dimensions are read at their smallest. A hole of nominal 20 mm (0.79 in) is therefore judged at its smallest diameter. For a part that fits an assembly, the cut size is the assembly size reduced by the limit deviation.

Prepared Edge

SSAB asks that thermal cut and sheared edges be deburred and rounded with a grinder before bending. It recommends removing them before the bend. An oxide edge on thick plate, at the outside of a tight bend, starts cracks sooner than a clean one. Dressing the edge also removes burrs that stop panels from seating flat for welding.

Fit Stack

A feature built on a cut edge stacks several errors. On 2 mm (0.079 in) sheet, range 2 squareness allows 0.164 mm (0.0065 in). Normal cold rolled thickness tolerance adds ±0.10 mm (±0.004 in). Together they reach about 0.26 mm (0.010 in) before any size error. A fit window of 0.3 mm (0.012 in) cannot be held by that stack with margin. Critical features are therefore dimensioned to each other within one cut.

Next Process

The edge a part needs depends on what follows the cut. A painted or galvanized part needs the oxide removed, or a nitrogen cut. An edge welded as cut carries its oxide into the pool. Edges that mate need their burr removal stated, with the radius or feel accepted. The approved first piece then sets the edge that every later batch has to match.

Reading Zone

ISO 9013 does not read the whole face. It excludes a zone at the upper and lower edges to allow for the melting of the top edge. Up to 3 mm (0.12 in) that zone is 0.1 times the thickness at each edge. On 2 mm (0.079 in) sheet, squareness is therefore read on 1.6 mm (0.063 in) of the face. Readings near the start and end of the cut, at small radii and at sharp angles fall outside the classes. Dross or melted drops at the lower edge are recorded as additional characteristics.

Sheet Metal Inspection From First Article to Batch Release

Measure the first part against every requirement, then release each lot on a defined sample, with weld, coating and hardware checks tied to their standards.

First Article Inspection for Sheet Metal PartsA first article inspection measures the first part made by the production process against every requirement on the drawing and records the result. In aerospace the practice has its own standard, SAE AS9102, whose scope is to establish the baseline requirements for performing and documenting a first article inspection.

Minimum Bend Radius by Sheet Material and Thickness

Take the minimum bend radius from the maker's table for the exact grade, temper, thickness and bend direction, then draw the radius the die forms.

Minimum Inside Bend Radius Values for Steel SheetSteel makers print the minimum as a multiple of thickness, t, and the multiple rises with strength and with thickness. The two hot-rolled cold-forming ranges below are the clearest published sets; mild cold-rolled steels such as DC01 come with formability figures but, in the makers' datasheets cited here, no printed radius.

ISO 2768 and DIN 6930 General Tolerances for Bent Sheet Metal Parts

ISO 2768-1 covers sheet metal parts by size class; on a bent part its angular row decides fit, and DIN 6930-2 is written for stamped steel parts only.

What ISO 2768-1 Covers on a Sheet Metal DrawingISO 2768-1, first edition 1989-11-15, sets general tolerances for linear and angular dimensions without individual tolerance indications, in four classes. Its scope names sheet metal directly: it applies to the dimensions of parts produced by metal removal or parts formed from sheet metal.

ISO 1461 Hot-Dip Galvanizing of Fabricated Steel Parts

ISO 1461 sets zinc thickness by steel thickness, measures it away from edges, and expects cut edges ground and parts bent before galvanizing.

What ISO 1461 Covers for Cut and Bent Steel PartsISO 1461:2022, the fourth edition, sets out the properties and test methods of zinc coatings formed when finished iron and steel articles, some castings included, are dipped in molten zinc holding at most 2 % of other metals. Its key word is fabricated: the parts are cut, formed and welded first and galvanized afterward in batches, by a company the standard now defines as the galvanizer.

High-Strength Steel Sheet S355 and S420 and the Springback It Brings

Order S355 or S420 for bent parts as the EN 10149-2 MC grade, bend at the recommended radius, and expect more springback than mild steel.

S355 and S420 Sheet Grades in EN 10149-2 and EN 10025-2High-strength sheet for cut and bent parts comes mainly from two European product standards. EN 10025-2 covers non-alloy structural steels, the S235, S275 and S355 families with the JR, J0 and J2 suffixes that set the impact-test temperature.

Cold Rolled DC01 and Hot Rolled S235 Steel Sheet for Cut and Bent Parts

Choose DC01 for thin formed parts that need tight thickness, flatness and a clean surface, and S235 for thicker load-bearing parts, then name the standard on the order.

DC01 and S235 Compared for Laser Cut and Bent Sheet PartsDC01 is a cold-rolled non-alloy mild steel for cold forming under EN 10130, material number 1.0330, which ArcelorMittal describes as having a guaranteed maximum yield and tensile strength, a guaranteed minimum elongation and good formability. S235 is a hot-rolled carbon-manganese structural steel under EN 10025-2, described by the same mill as having a guaranteed minimum yield and tensile strength and satisfactory ductility, in JR, J0 and J2 versions that differ in impact-test temperature.

Press Brake Bending of Sheet Metal From Die Opening to Final Angle

A press brake bend is decided by the die opening, which sets radius, flange length, springback and the flat pattern, so the first piece carries every assumption of the lot.

How a Press Brake Forms a Bend in AirMost sheet metal is bent by air forming. The punch pushes the sheet into a V-shaped die, and the sheet touches only three points: the two shoulders of the die and the tip of the punch.

Laser Cutting Sheet Metal With Oxygen, Nitrogen or Air Assist Gas

Oxygen, nitrogen and air each leave a different edge on laser cut sheet, and the choice of gas settles speed, finishing work and what the next process accepts.

Which Assist Gas Cuts Which Sheet MetalThree gases cover almost all sheet work: oxygen, nitrogen and compressed air. Oxygen belongs to carbon and low-alloy steel, nitrogen to stainless steel and aluminum, and air sits between them as the cheaper trade for thin parts that tolerate a slightly darker edge.

Laser Cut Part Dimensional Tolerance Under ISO 9013 Class 1 and Class 2

Pick the tighter or looser dimensional class per feature, read inside and outside sizes at their extremes, and anchor fit features to each other.

What Dimensional Tolerance Class 1 and Class 2 Cover on a Laser Cut PartISO 9013:2017 applies to laser cuts from 0.5 mm to 32 mm in thickness. Its clause 8 gives limit deviations for nominal dimensions in two classes, listed in Table 6 for class 1 and Table 7 for class 2.

Cold Rolled Steel Sheet Thickness Tolerance Under EN 10131

Choose the tolerance column by what the part does with a thickness error, and write the strength class and column on the order.

What EN 10131 Allows on the Thickness of a Cold Rolled SheetEN 10131 covers cold rolled flat products of uncoated and electrolytically coated steel, and ArcelorMittal's tolerance tables reproduce its thickness limits as guarantees. The tables run from 0.35 mm to 3.00 mm and apply per nominal thickness band, per width class and per yield strength class.

ISO 9013 Laser Cut Edge Quality Ranges for Squareness and Roughness

Pick a squareness range and a roughness range by thickness, add the dimensional class, and agree how thin sheet is measured.

What the ISO 9013 Ranges Tell You About a Laser Cut EdgeISO 9013:2017 presents geometrical product specifications and quality tolerances for thermal cuts in materials suitable for oxyfuel flame cutting, plasma cutting and laser cutting. Its scope runs from 3 mm to 300 mm for flame cuts, 0.5 mm to 150 mm for plasma cuts and 0.5 mm to 32 mm for laser cuts.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.