Bending

Bending forms sheet into an angle along a straight line, stretching the outside of the bend and compressing the inside.

Every Bending article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Bending forms sheet into an angle along a straight line, stretching the outside of the bend and compressing the inside. Most sheet is bent on a press brake by air forming. Progressive dies bend in stations instead. Thickness, grade, grain and the cut edge all change the result.

Air Forming

In air forming the punch presses the sheet into a V die. The sheet touches only the two die shoulders and the punch tip. Ram travel, not the groove, sets the angle, so one die serves many angles. Wila notes that the die opening sets the inside radius. Bottoming and coining force the sheet deeper and need more tonnage.
Read More

Force Estimate

Durma gives bending force as bend length times thickness squared times tensile strength times 1.42, over the V opening. Take 1,000 mm (39 in) of 2 mm (0.079 in) mild steel over a 16 mm (0.63 in) die. The estimate is about 160 kN (36,000 lbf). Doubling the V opening roughly halves the force. Stainless takes 1.4 to 1.5 times mild steel, and 5052 aluminum 0.5 to 0.6 times. Euro Inox puts austenitic stainless about 50 % above carbon steel of similar thickness.

Material Response

Each grade answers the bend differently. Austenitic stainless work hardens as it deforms, so a second bend in the same area meets harder metal. Cleveland-Cliffs notes that 316 hardens more slowly than 304 because of its higher nickel. In 5052, the H32 temper sits between soft O and full-hard H38 in strength and ductility. The Fabricator’s column works with a tensile strength about a quarter higher for 5052-H38 than for H32, and the minimum radius rises with it.

Grain Direction

Rolled sheet bends differently along and across its grain. SSAB notes that grains run along the rolling direction, so a bend across it survives a tighter radius. Across the grain, a tighter radius survives. A nest of bent parts therefore locks their bend lines to the rolling direction.

Thickness Effect

Sheet thickness changes how far metal stretches at the bend. Flange length and final angle therefore shift with the thickness band of the sheet. No tolerance table quantifies that shift. The first formed piece from the actual sheet is where it is found. Three layers stacked in a hem can carry three thickness bands at once.

Surface Effects

Some finishes survive the bend and some change with it. Electrolytic coloring on stainless survives bending, though the film thins and the color deepens less at the bend. Witness marks along the bend line come from a narrow die or sharp shoulders. Fine cracks or orange-peel texture on the outer radius point to too tight a radius or the wrong grain direction.

First Bend

The first piece carries every assumption of the setup. Its angle is measured at both ends of each bend. Its outer radius is read at ten times magnification for cracks. The die width, punch radius, control angle and K-factor are recorded with it. A second piece from the far end of the lot shows whether the first was luck.

Flat Pattern Link

The bend also sets the length of the blank cut before it. Durma gives the bend allowance from the angle, inside radius, thickness and K-factor. Its reference K runs from 0.33 for a tight air bend to 0.50 above three thicknesses of radius. Wila warns that changing the V opening changes the flat pattern, which is costly to correct once parts are cut. The shop records die, punch and K-factor with the material lot for the next run.

Minimum Bend Radius by Sheet Material and Thickness

Take the minimum bend radius from the maker's table for the exact grade, temper, thickness and bend direction, then draw the radius the die forms.

Minimum Inside Bend Radius Values for Steel SheetSteel makers print the minimum as a multiple of thickness, t, and the multiple rises with strength and with thickness. The two hot-rolled cold-forming ranges below are the clearest published sets; mild cold-rolled steels such as DC01 come with formability figures but, in the makers' datasheets cited here, no printed radius.

Bend Angle and Flange Length Tolerance on Press Brake Parts

Set the bend angle tolerance from the position the flange tip has to reach, and control sheet thickness, die width and the flat pattern behind it.

Bend Angle and Flange Length Tolerance ValuesThere is no single tolerance for bent sheet metal. Durmapress says so plainly and offers planning ranges per operation instead, warning that they are a guide only and move with the material, thickness, size of part, machine, state of the tooling, number of operations and the way parts are inspected.

ISO 2768 and DIN 6930 General Tolerances for Bent Sheet Metal Parts

ISO 2768-1 covers sheet metal parts by size class; on a bent part its angular row decides fit, and DIN 6930-2 is written for stamped steel parts only.

What ISO 2768-1 Covers on a Sheet Metal DrawingISO 2768-1, first edition 1989-11-15, sets general tolerances for linear and angular dimensions without individual tolerance indications, in four classes. Its scope names sheet metal directly: it applies to the dimensions of parts produced by metal removal or parts formed from sheet metal.

ISO 1461 Hot-Dip Galvanizing of Fabricated Steel Parts

ISO 1461 sets zinc thickness by steel thickness, measures it away from edges, and expects cut edges ground and parts bent before galvanizing.

What ISO 1461 Covers for Cut and Bent Steel PartsISO 1461:2022, the fourth edition, sets out the properties and test methods of zinc coatings formed when finished iron and steel articles, some castings included, are dipped in molten zinc holding at most 2 % of other metals. Its key word is fabricated: the parts are cut, formed and welded first and galvanized afterward in batches, by a company the standard now defines as the galvanizer.

High-Strength Steel Sheet S355 and S420 and the Springback It Brings

Order S355 or S420 for bent parts as the EN 10149-2 MC grade, bend at the recommended radius, and expect more springback than mild steel.

S355 and S420 Sheet Grades in EN 10149-2 and EN 10025-2High-strength sheet for cut and bent parts comes mainly from two European product standards. EN 10025-2 covers non-alloy structural steels, the S235, S275 and S355 families with the JR, J0 and J2 suffixes that set the impact-test temperature.

Progressive Die Stamping After Laser Cut and Bent Sheet Metal Parts

A progressive die makes parts in minutes but takes months to build and wants a design that has stopped, so quantity and design stability choose between die and laser.

What Changes When a Part Moves From Laser and Brake to a DieIn laser and brake work, a flat blank is cut by a beam from a program and bent on a press brake with standard tooling, so a part exists the day the drawing and the sheet exist. In progressive stamping, a continuous strip passes through one die set with several stations.

Press Brake Bending of Sheet Metal From Die Opening to Final Angle

A press brake bend is decided by the die opening, which sets radius, flange length, springback and the flat pattern, so the first piece carries every assumption of the lot.

How a Press Brake Forms a Bend in AirMost sheet metal is bent by air forming. The punch pushes the sheet into a V-shaped die, and the sheet touches only three points: the two shoulders of the die and the tip of the punch.

Cold Rolled Steel Sheet Thickness Tolerance Under EN 10131

Choose the tolerance column by what the part does with a thickness error, and write the strength class and column on the order.

What EN 10131 Allows on the Thickness of a Cold Rolled SheetEN 10131 covers cold rolled flat products of uncoated and electrolytically coated steel, and ArcelorMittal's tolerance tables reproduce its thickness limits as guarantees. The tables run from 0.35 mm to 3.00 mm and apply per nominal thickness band, per width class and per yield strength class.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

316L Stainless Steel Sheet for Laser Cutting and Bending

Choose the molybdenum-bearing low-carbon grade for chloride exposure, plan overbend on the brake, and write the finish and weld tint rules on the drawing.

What 316L Sheet Adds Over 304L in a Cut and Bent PartType 316L is Type 316 with the carbon ceiling lowered from 0.08 % to 0.03 % by weight. Both carry 16.0 to 18.0 % chromium, 10.0 to 14.0 % nickel and 2.00 to 3.00 % molybdenum, according to the Cleveland-Cliffs product bulletin for the two types.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote