Aluminum

Aluminum sheet weighs about a third as much as stainless at equal thickness, and 5052 is an aluminum-magnesium alloy used for bent and welded parts.

Every Aluminum article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Aluminum sheet weighs about a third as much as stainless at equal thickness, and 5052 is an aluminum-magnesium alloy used for bent and welded parts. At the Aluminum Association’s nominal density of 2.68 g/cm³, 2 mm (0.079 in) of 5052 weighs about 5.4 kg/m² (1.1 lb/ft²). The same thickness of 316L weighs 16.1 kg/m² (3.3 lb/ft²). Alloy 5052 cannot be hardened by heat treatment, so its strength comes from cold work. The temper code, H32 for quarter hard, records how much.

Stiffness Trade

Weight is only half of the comparison. Smiths lists 5052 at 70 GPa (10,200 ksi), and Cleveland-Cliffs lists 316L at 193 GPa (28,000 ksi). At equal thickness the aluminum panel is about 36 % as stiff. Matching a 2 mm (0.079 in) stainless panel takes 2.8 mm (0.110 in) of 5052. That thicker panel weighs 7.6 kg/m² (1.6 lb/ft²), about 47 % of the stainless one. The thicker sheet then needs a larger bend radius, so the saving is paid for in geometry.
Read More

Grades and Bases

Three 5052 H32 datasheets print three minimum yields, and none of them is wrong. Smiths lists 175 MPa (25 ksi) without naming a basis. The Aluminum Association’s register shows 5251 with less magnesium, 1.7 to 2.4 %, so a substitute alloy is named on the order if it is accepted. The governing specification on the order is what settles the number.

Cut Surface

ISO 9013 treats the cut face of aluminum as a special case. Annex A says aluminum, titanium, magnesium and copper alloys show rippled faces that depend on grain structure. On those faces Rz5 cannot be determined and evaluated by the standard. For aluminum it says to expect values about four times its ranges. A drawing therefore states squareness as a number and agrees the edge look with a sample. Air Liquide notes that air leaves more dross on aluminum than nitrogen does.

Cutting Speed

GWEIKE’s nitrogen tables run thin aluminum close to stainless speeds. They list 3 mm (0.12 in) aluminum at 14 to 16 m/min (550 to 630 in/min) on 6 kW. On 12 kW the same sheet runs at 25 to 30 m/min (985 to 1,180 in/min). Pressure starts near 12 bar (174 psi) and rises to 18 to 20 bar (261 to 290 psi) from 10 mm (0.39 in). TRUMPF lists 25 mm (0.98 in) as the thickest aluminum cut on its 6 kW machines.

Forming Force

Aluminum takes a narrower die and less force than steel. Durma puts the V opening for 5052 at 5 to 6 thicknesses, against about 8 for mild steel. The formed inside radius comes out at 13 to 15 % of that opening. Bending force for 5052 is 0.5 to 0.6 times that of mild steel in Durma’s factors. The harder 6061-T6 wants an opening of 10 to 12 thicknesses. A bending column in The Fabricator charts 0 to 1 t for 3.2 mm (0.125 in) 5052-H32, against a supplier’s suggestion of 1.5 t quoted in the same column.

Welding Window

Lincoln Electric notes that 5xxx alloys are arc weldable by TIG and MIG, and ESAB warns that 5052 cracks with a base-alloy filler, so 5356 is the usual choice. The common fillers are 4043 and 5356, chosen for the alloys being joined. Smiths prints a thermal expansion of 23.7 x 10⁻⁶ per kelvin without a temperature range. At face value, a 1,000 mm (39.4 in) edge grows 0.24 mm (0.009 in) for every 10 K (18 °F). ISO 5817 covers steel, nickel and titanium, so an aluminum seam needs another quality document. The 5052 datasheets do not say how much H32 strength survives beside a weld.

Coating Pretreatment

IGP’s powder data sheet lists chromating to DIN EN 12487 as one aluminum pretreatment. The others are pre-anodizing and a chrome-free system to GSB International and QUALICOAT specifications. For aluminum and galvanized parts, a boiling water test with a cross-cut adhesion and tape test is the minimum check. Euro Inox adds that stainless is more noble than aluminum. A stainless fixing in an aluminum part therefore needs a nylon or neoprene barrier. The aluminum data sheets print no flatness value, so a flat panel is asked for by number.

Inserting Self-Clinching Fasteners in Sheet Metal Step by Step

Cut the hole to size without deburring, check the sheet is soft enough, finish the panel, then squeeze the nut in parallel until its head meets the sheet.

How a Self-Clinching Nut Locks Into Thin SheetInstallation takes three moves. First a hole of the specified size is punched or drilled, the nut's shank is placed in it, and a press squeezes nut and sheet between parallel surfaces until the head meets the sheet.

Minimum Bend Radius by Sheet Material and Thickness

Take the minimum bend radius from the maker's table for the exact grade, temper, thickness and bend direction, then draw the radius the die forms.

Minimum Inside Bend Radius Values for Steel SheetSteel makers print the minimum as a multiple of thickness, t, and the multiple rises with strength and with thickness. The two hot-rolled cold-forming ranges below are the clearest published sets; mild cold-rolled steels such as DC01 come with formability figures but, in the makers' datasheets cited here, no printed radius.

Bend Angle and Flange Length Tolerance on Press Brake Parts

Set the bend angle tolerance from the position the flange tip has to reach, and control sheet thickness, die width and the flat pattern behind it.

Bend Angle and Flange Length Tolerance ValuesThere is no single tolerance for bent sheet metal. Durmapress says so plainly and offers planning ranges per operation instead, warning that they are a guide only and move with the material, thickness, size of part, machine, state of the tooling, number of operations and the way parts are inspected.

ISO 2768 and DIN 6930 General Tolerances for Bent Sheet Metal Parts

ISO 2768-1 covers sheet metal parts by size class; on a bent part its angular row decides fit, and DIN 6930-2 is written for stamped steel parts only.

What ISO 2768-1 Covers on a Sheet Metal DrawingISO 2768-1, first edition 1989-11-15, sets general tolerances for linear and angular dimensions without individual tolerance indications, in four classes. Its scope names sheet metal directly: it applies to the dimensions of parts produced by metal removal or parts formed from sheet metal.

Powder Coated Sheet Metal Batch From Pretreatment to Cure and Inspection

A powder coating cures in minutes but depends on pretreatment, rack mass and film allowance, and a lot is judged on gloss, film and adhesion, not corrosion hours.

The Stages a Coated Batch Passes ThroughA batch of sheet metal parts goes through six stages on its way from the bare part to a coated one: pretreatment, drying, masking and hanging, application, cure, and cooling and packing. Each stage has a condition the powder maker states, and each has its own place in the schedule.

Press Brake Bending of Sheet Metal From Die Opening to Final Angle

A press brake bend is decided by the die opening, which sets radius, flange length, springback and the flat pattern, so the first piece carries every assumption of the lot.

How a Press Brake Forms a Bend in AirMost sheet metal is bent by air forming. The punch pushes the sheet into a V-shaped die, and the sheet touches only three points: the two shoulders of the die and the tip of the punch.

Laser Cutting Sheet Metal With Oxygen, Nitrogen or Air Assist Gas

Oxygen, nitrogen and air each leave a different edge on laser cut sheet, and the choice of gas settles speed, finishing work and what the next process accepts.

Which Assist Gas Cuts Which Sheet MetalThree gases cover almost all sheet work: oxygen, nitrogen and compressed air. Oxygen belongs to carbon and low-alloy steel, nitrogen to stainless steel and aluminum, and air sits between them as the cheaper trade for thin parts that tolerate a slightly darker edge.

Steel Sheet Flatness Tolerance Before Cutting and Bending

Read flatness by thickness, width and strength class, specify normal or special, and keep parts clear of the edge wave strip.

What a Flatness Tolerance Covers Before the First CutIn the EN 10131 and EN 10051 tables, as ArcelorMittal prints them, flatness is a maximum deviation in millimeters, and the tables apply to sheet, not to coil. The extract does not describe the set-up used to measure it.

ISO 9013 Laser Cut Edge Quality Ranges for Squareness and Roughness

Pick a squareness range and a roughness range by thickness, add the dimensional class, and agree how thin sheet is measured.

What the ISO 9013 Ranges Tell You About a Laser Cut EdgeISO 9013:2017 presents geometrical product specifications and quality tolerances for thermal cuts in materials suitable for oxyfuel flame cutting, plasma cutting and laser cutting. Its scope runs from 3 mm to 300 mm for flame cuts, 0.5 mm to 150 mm for plasma cuts and 0.5 mm to 32 mm for laser cuts.

ISO 5817 Weld Quality Levels B, C and D for Sheet Metal Parts

Name a quality level per joint, cite the current edition, and agree how thin-sheet welds are inspected and finished.

What Quality Levels B, C and D Mean for a Sheet Metal WeldISO 5817 specifies quality levels for imperfections in fusion-welded joints in steel, nickel, titanium and their alloys. It applies to material 0.5 mm thick and above and covers fully penetrated butt welds and all fillet welds.

Galvanized Steel Sheet Coating Weight Designations for Cut and Welded Parts

Read the coating designation as a minimum zinc mass over both faces, name the standard and test basis, and plan ventilation for cutting and welding.

What a Coating Weight Designation Says About the SheetA designation states the minimum mass of zinc, or zinc alloy, on the sheet and the units it is stated in. G90 means hot-dip galvanized, with a triple spot test average of at least 0.90 ounce per square foot, counted over both sides together.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote