Joint

A joint is where two sheet parts meet and are held, by a weld, a lap, a hem or a tab in a slot.

Every Joint article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A joint is where two sheet parts meet and are held, by a weld, a lap, a hem or a tab in a slot. Its quality depends on the gap, the thickness of each part and the method that closes it. In ISO 5817 the joint, not the whole product, is the unit that receives a quality level. One part can therefore carry different levels on different joints.

Level per Joint

ISO 5817 lets a drawing give one level for the whole part and another for the joints that need it. An enclosure seam that is ground flush and painted may take level C. A pressure-bearing or fatigue-loaded joint may call for level B, with the rest at D. The standard asks for the choice before production starts.
Read More

Gap and Fit-Up

Most distortion is settled before the first seam, by the way the joint is assembled. TWI says tack welds set and hold the joint gap and resist transverse shrinkage. With too few tacks, the joint closes up as welding proceeds. On thick plate cut by laser, ISO 9013 sets the cut size as the assembly size reduced by the limit deviation. The gap is then a number the designer chose.

Thickness Stack

A joint that stacks layers adds their thickness bands. Three layers of 2 mm (0.079 in) cold rolled sheet on normal tolerance can carry 0.30 mm (0.012 in) of excess or shortfall. On galvanized sheet, the zinc adds to the stack, so the drawing says whether the nominal is bare or coated. A tab joint cut to the bare value meets a coated sheet up to the coating thickness thicker.

Joint Strength

A welded aluminum joint has no catalog strength in the 5052 datasheets. A drawing that relies on the full H32 yield across such a joint asks a question the sheets do not answer. The load the joint carries therefore goes on the drawing, so a strength test is planned. ISO 5817 itself does not cover fitness for purpose, apart from its fatigue annex.

Sheet Metal Inspection From First Article to Batch Release

Measure the first part against every requirement, then release each lot on a defined sample, with weld, coating and hardware checks tied to their standards.

First Article Inspection for Sheet Metal PartsA first article inspection measures the first part made by the production process against every requirement on the drawing and records the result. In aerospace the practice has its own standard, SAE AS9102, whose scope is to establish the baseline requirements for performing and documenting a first article inspection.

Inserting Self-Clinching Fasteners in Sheet Metal Step by Step

Cut the hole to size without deburring, check the sheet is soft enough, finish the panel, then squeeze the nut in parallel until its head meets the sheet.

How a Self-Clinching Nut Locks Into Thin SheetInstallation takes three moves. First a hole of the specified size is punched or drilled, the nut's shank is placed in it, and a press squeezes nut and sheet between parallel surfaces until the head meets the sheet.

Bend Angle and Flange Length Tolerance on Press Brake Parts

Set the bend angle tolerance from the position the flange tip has to reach, and control sheet thickness, die width and the flat pattern behind it.

Bend Angle and Flange Length Tolerance ValuesThere is no single tolerance for bent sheet metal. Durmapress says so plainly and offers planning ranges per operation instead, warning that they are a guide only and move with the material, thickness, size of part, machine, state of the tooling, number of operations and the way parts are inspected.

ISO 1461 Hot-Dip Galvanizing of Fabricated Steel Parts

ISO 1461 sets zinc thickness by steel thickness, measures it away from edges, and expects cut edges ground and parts bent before galvanizing.

What ISO 1461 Covers for Cut and Bent Steel PartsISO 1461:2022, the fourth edition, sets out the properties and test methods of zinc coatings formed when finished iron and steel articles, some castings included, are dipped in molten zinc holding at most 2 % of other metals. Its key word is fabricated: the parts are cut, formed and welded first and galvanized afterward in batches, by a company the standard now defines as the galvanizer.

Laser Cut Part Dimensional Tolerance Under ISO 9013 Class 1 and Class 2

Pick the tighter or looser dimensional class per feature, read inside and outside sizes at their extremes, and anchor fit features to each other.

What Dimensional Tolerance Class 1 and Class 2 Cover on a Laser Cut PartISO 9013:2017 applies to laser cuts from 0.5 mm to 32 mm in thickness. Its clause 8 gives limit deviations for nominal dimensions in two classes, listed in Table 6 for class 1 and Table 7 for class 2.

Cold Rolled Steel Sheet Thickness Tolerance Under EN 10131

Choose the tolerance column by what the part does with a thickness error, and write the strength class and column on the order.

What EN 10131 Allows on the Thickness of a Cold Rolled SheetEN 10131 covers cold rolled flat products of uncoated and electrolytically coated steel, and ArcelorMittal's tolerance tables reproduce its thickness limits as guarantees. The tables run from 0.35 mm to 3.00 mm and apply per nominal thickness band, per width class and per yield strength class.

ISO 5817 Weld Quality Levels B, C and D for Sheet Metal Parts

Name a quality level per joint, cite the current edition, and agree how thin-sheet welds are inspected and finished.

What Quality Levels B, C and D Mean for a Sheet Metal WeldISO 5817 specifies quality levels for imperfections in fusion-welded joints in steel, nickel, titanium and their alloys. It applies to material 0.5 mm thick and above and covers fully penetrated butt welds and all fillet welds.

Galvanized Steel Sheet Coating Weight Designations for Cut and Welded Parts

Read the coating designation as a minimum zinc mass over both faces, name the standard and test basis, and plan ventilation for cutting and welding.

What a Coating Weight Designation Says About the SheetA designation states the minimum mass of zinc, or zinc alloy, on the sheet and the units it is stated in. G90 means hot-dip galvanized, with a triple spot test average of at least 0.90 ounce per square foot, counted over both sides together.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote