A weld is the joint made by fusing sheet edges or faces together, as a butt seam, a fillet or a resistance spot.

Every Weld article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A weld is the joint made by fusing sheet edges or faces together, as a butt seam, a fillet or a resistance spot. In sheet work its acceptance comes from a quality standard, and its shape comes from the sequence and the heat. The two are separate questions on the drawing. A seam can meet its quality level and still leave a panel out of square.

Quality Level

ISO 5817 grades fusion welds in steel, nickel and titanium from 0.5 mm (0.02 in) thick. Its three levels are D, C and B, with B the strictest. A level applies to a joint, not to a whole product, so one part can carry several levels. Level B values may need grinding or TIG dressing, the standard’s introduction notes. Laser and electron beam welds fall under ISO 13919-1 instead. Aluminum is outside the scope, so a 5052 seam takes its level from an aluminum weld standard.
Read More

Heat and Shrinkage

Weld metal shrinks as it cools, and the cold sheet around it gives way. TWI names three results: angular distortion, longitudinal shrinkage and transverse shrinkage. Tack welds set the joint gap and resist the transverse pull. Back-step and skip sequences place each short length where the panel is cool. TWI also asks for fillets at the specified minimum size, since every extra millimeter is more shrinkage. A spot weld on steel runs at 8 to 15 kA for about a fifth of a second, per AHSS Insights.

Edge Preparation

A weld starts at a cut edge, and the edge brings its own condition. A laser cut in oxygen leaves an oxide layer that enters the weld pool unless it is cleaned. A nitrogen cut leaves a bright, scale-free edge that goes to the torch as it is. SSAB asks that thermal cut edges be deburred and rounded with a grinder. On thick plate, ISO 9013 says the nominal size of a cut part is the assembly size reduced by the limit deviation. The joint gap is then a number the designer chose.

Filler Choice

The filler follows the base metal. Cleveland-Cliffs names AWS 308, 308L or 347 for 304, and 316L or 16-8-2 for 316. It asks for ferrite in the deposit to avoid hot cracking. For 5052 aluminum, Lincoln Electric names 4043, 5554 or 5356, chosen for the alloys being joined. A welding procedure is qualified for a thickness band. A shop qualified on 1.5 mm (0.059 in) stainless therefore holds a different qualification from one welding 6 mm (0.24 in).

Surface Aftercare

Some weld results have no fixed limit at any ISO 5817 level. Spatter and temper colors are accepted by the application, so the drawing states them. On a directional stainless finish, the finish is restored at the welded junction, per Euro Inox. Electrolytically colored stainless cannot be welded without destroying its color. On galvanized sheet, zinc oxide fume from welding is the common cause of metal fume fever. The AWS fact sheet points to local exhaust at the arc as the first control.

Strength Basis

A weld’s strength is not always printed anywhere. The 5052 data sheets leave the strength beside a weld unstated. A load-bearing aluminum joint therefore rests on a strength test, not a catalog number. ISO 5817 Annex B adds fatigue designations such as B90 and C63 for steel. Its footnote says they were proved for 10 mm (0.39 in) and above, so thin sheet treats them as a starting point.

Checking the Part

A welded assembly is checked in the order it was built: size, then squareness, then flatness and hole position. Equal diagonals show that a box is square. Flatness is read with the part resting free on a surface plate, not clamped. Holes are checked after welding, since a hole that fit before can move.

Sheet Metal Inspection From First Article to Batch Release

Measure the first part against every requirement, then release each lot on a defined sample, with weld, coating and hardware checks tied to their standards.

First Article Inspection for Sheet Metal PartsA first article inspection measures the first part made by the production process against every requirement on the drawing and records the result. In aerospace the practice has its own standard, SAE AS9102, whose scope is to establish the baseline requirements for performing and documenting a first article inspection.

ISO 1461 Hot-Dip Galvanizing of Fabricated Steel Parts

ISO 1461 sets zinc thickness by steel thickness, measures it away from edges, and expects cut edges ground and parts bent before galvanizing.

What ISO 1461 Covers for Cut and Bent Steel PartsISO 1461:2022, the fourth edition, sets out the properties and test methods of zinc coatings formed when finished iron and steel articles, some castings included, are dipped in molten zinc holding at most 2 % of other metals. Its key word is fabricated: the parts are cut, formed and welded first and galvanized afterward in batches, by a company the standard now defines as the galvanizer.

Laser Cutting Sheet Metal With Oxygen, Nitrogen or Air Assist Gas

Oxygen, nitrogen and air each leave a different edge on laser cut sheet, and the choice of gas settles speed, finishing work and what the next process accepts.

Which Assist Gas Cuts Which Sheet MetalThree gases cover almost all sheet work: oxygen, nitrogen and compressed air. Oxygen belongs to carbon and low-alloy steel, nitrogen to stainless steel and aluminum, and air sits between them as the cheaper trade for thin parts that tolerate a slightly darker edge.

Laser Cut Part Dimensional Tolerance Under ISO 9013 Class 1 and Class 2

Pick the tighter or looser dimensional class per feature, read inside and outside sizes at their extremes, and anchor fit features to each other.

What Dimensional Tolerance Class 1 and Class 2 Cover on a Laser Cut PartISO 9013:2017 applies to laser cuts from 0.5 mm to 32 mm in thickness. Its clause 8 gives limit deviations for nominal dimensions in two classes, listed in Table 6 for class 1 and Table 7 for class 2.

ISO 5817 Weld Quality Levels B, C and D for Sheet Metal Parts

Name a quality level per joint, cite the current edition, and agree how thin-sheet welds are inspected and finished.

What Quality Levels B, C and D Mean for a Sheet Metal WeldISO 5817 specifies quality levels for imperfections in fusion-welded joints in steel, nickel, titanium and their alloys. It applies to material 0.5 mm thick and above and covers fully penetrated butt welds and all fillet welds.

Galvanized Steel Sheet Coating Weight Designations for Cut and Welded Parts

Read the coating designation as a minimum zinc mass over both faces, name the standard and test basis, and plan ventilation for cutting and welding.

What a Coating Weight Designation Says About the SheetA designation states the minimum mass of zinc, or zinc alloy, on the sheet and the units it is stated in. G90 means hot-dip galvanized, with a triple spot test average of at least 0.90 ounce per square foot, counted over both sides together.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

316L Stainless Steel Sheet for Laser Cutting and Bending

Choose the molybdenum-bearing low-carbon grade for chloride exposure, plan overbend on the brake, and write the finish and weld tint rules on the drawing.

What 316L Sheet Adds Over 304L in a Cut and Bent PartType 316L is Type 316 with the carbon ceiling lowered from 0.08 % to 0.03 % by weight. Both carry 16.0 to 18.0 % chromium, 10.0 to 14.0 % nickel and 2.00 to 3.00 % molybdenum, according to the Cleveland-Cliffs product bulletin for the two types.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote