ISO 5817

ISO 5817 is the international standard that sets quality levels B, C and D for imperfections in fusion welds in steel, nickel and titanium.

Every ISO 5817 article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

ISO 5817 is the international standard that sets quality levels B, C and D for imperfections in fusion welds in steel, nickel and titanium. It applies from 0.5 mm (0.02 in) thickness, to fully penetrated butt welds and all fillet welds. Its fourth edition is dated 2023. Level B is the strictest.

Scope

The standard covers manual, mechanized and automatic welding in all positions. Its processes, by ISO 4063 number, include metal arc, submerged arc, gas-shielded metal arc, TIG, plasma arc and oxyfuel welding of steel. Laser and electron beam welds are excluded and sent to ISO 13919-1. Aluminum is outside the scope, so an aluminum seam needs another document. Metallurgical aspects such as grain size and hardness are not covered.
Read More

Thin Material

For 0.5 to 3 mm (0.02 to 0.12 in), most limits are fractions of the thickness t. Level C allows undercut to 0.1 t, which is 0.15 mm (0.006 in) on 1.5 mm (0.059 in) sheet. Level B allows no short undercut, groove, concavity or sagging. Several imperfections in one cross-section are not permitted at any level in that band.

What It Leaves Open

The standard does not choose a level for a product. That choice falls to the application standard or the designer, set before production. It leaves spatter and temper colors to the application at every level. It does not describe detection, and names ISO 17635 for the non-destructive methods.

Fatigue Annex

Annex B adds fatigue-extended levels: C63, B90 and B125. B125 is generally not achieved as welded and excludes fillet welds. A footnote says the values were proved for 10 mm (0.39 in) and above.

Drawing Use

A drawing names the edition, a level per joint and the inspection method. A drawing that cites an older edition may not describe the same inspection.

Sheet Metal Inspection From First Article to Batch Release

Measure the first part against every requirement, then release each lot on a defined sample, with weld, coating and hardware checks tied to their standards.

First Article Inspection for Sheet Metal PartsA first article inspection measures the first part made by the production process against every requirement on the drawing and records the result. In aerospace the practice has its own standard, SAE AS9102, whose scope is to establish the baseline requirements for performing and documenting a first article inspection.

ISO 5817 Weld Quality Levels B, C and D for Sheet Metal Parts

Name a quality level per joint, cite the current edition, and agree how thin-sheet welds are inspected and finished.

What Quality Levels B, C and D Mean for a Sheet Metal WeldISO 5817 specifies quality levels for imperfections in fusion-welded joints in steel, nickel, titanium and their alloys. It applies to material 0.5 mm thick and above and covers fully penetrated butt welds and all fillet welds.

Galvanized Steel Sheet Coating Weight Designations for Cut and Welded Parts

Read the coating designation as a minimum zinc mass over both faces, name the standard and test basis, and plan ventilation for cutting and welding.

What a Coating Weight Designation Says About the SheetA designation states the minimum mass of zinc, or zinc alloy, on the sheet and the units it is stated in. G90 means hot-dip galvanized, with a triple spot test average of at least 0.90 ounce per square foot, counted over both sides together.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

316L Stainless Steel Sheet for Laser Cutting and Bending

Choose the molybdenum-bearing low-carbon grade for chloride exposure, plan overbend on the brake, and write the finish and weld tint rules on the drawing.

What 316L Sheet Adds Over 304L in a Cut and Bent PartType 316L is Type 316 with the carbon ceiling lowered from 0.08 % to 0.03 % by weight. Both carry 16.0 to 18.0 % chromium, 10.0 to 14.0 % nickel and 2.00 to 3.00 % molybdenum, according to the Cleveland-Cliffs product bulletin for the two types.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote