MIG

MIG welding is the gas-shielded metal arc process, GMAW in Lincoln Electric's guide, which TWI prefers to manual metal arc for distortion.

Every MIG article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

MIG welding is the gas-shielded metal arc process, GMAW in Lincoln Electric’s guide, which TWI prefers to manual metal arc for distortion. ISO 5817 covers it as process 13. It suits mild steel and stainless sheet where speed matters. It also welds 5052 aluminum with 4043 or 5356 filler.

Distortion Control

TWI’s advice is to deposit weld metal quickly with the fewest runs. It recommends the largest wire or highest current that does not cause lack of fusion. Mechanized MIG, with high deposition at high travel speed, gives the most consistent distortion. That consistency is what makes presetting a part worth doing.
Read More

Materials

For 5052, Lincoln Electric names GMAW and GTAW as the arc processes, with argon at no less than 35 SCFH for MIG. The common fillers are 4043 and 5356, chosen for the alloys joined. Euro Inox lists MIG among the processes that suit stainless. For 316L, Cleveland-Cliffs names AWS E/ER 316L and 16-8-2 fillers.

Stainless Care

Stainless seams need care against hot cracking, with ferrite in the deposit. On a directional finish, the seam’s cleanup restores the finish at the junction.

Fusion Limit

TWI sets the upper bound of current and wire size at the highest setting that does not cause lack of fusion. ISO 5817 lists surface lack of fusion as not permitted at any level in sheet 0.5 mm (0.02 in) and thicker.

Quality Reference

A MIG seam in steel takes its quality level from ISO 5817. A MIG seam in 5052 takes it from an aluminum weld standard named on the drawing. A welding procedure is qualified for a thickness band, so the same MIG procedure does not carry across thicknesses.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

316L Stainless Steel Sheet for Laser Cutting and Bending

Choose the molybdenum-bearing low-carbon grade for chloride exposure, plan overbend on the brake, and write the finish and weld tint rules on the drawing.

What 316L Sheet Adds Over 304L in a Cut and Bent PartType 316L is Type 316 with the carbon ceiling lowered from 0.08 % to 0.03 % by weight. Both carry 16.0 to 18.0 % chromium, 10.0 to 14.0 % nickel and 2.00 to 3.00 % molybdenum, according to the Cleveland-Cliffs product bulletin for the two types.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote