Residual Stress

Residual stress is stress held inside a sheet or a weld, released when material is cut away and able to move the part.

Every Residual Stress article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Residual stress is stress held inside a sheet or a weld, released when material is cut away and able to move the part. ISO 9013 names its relaxation as a reason laser tolerances depend on material and temperature. It can bow a part after it leaves the skeleton. Welding adds its own residual stress, held in place by clamps until they open.

During Cutting

ISO 9013 states that material grade and sheet temperature, set against machine temperature, have to suit the sheet’s movement. That movement is the elongation or contraction that comes as residual stress relaxes and the sheet heats. The dimensional classes assume that condition is met. With stainless at 16.0 µm/m/K (8.9 µin/in/°F), a long, narrow part cut in one hot pass is the shape that moves.
Read More

After Release

Cutting releases stress as material is taken away. A part cut from a stressed sheet can move after it leaves the skeleton. The movement depends on the nest layout, not on the nominal flatness of the sheet. No table answers that, so a first article is the test.

In Flatness

One reading of the EN 10131 flatness table is that thin sheet takes the shape of its own residual stresses. The standard does not state that reason.

In Welding

A clamped panel cannot move, so weld shrinkage stays in the metal as stress. It comes out when the clamps are removed. TWI recommends stress relieving back-to-back assemblies before they are separated. Measuring a part in the fixture and again out of it shows how much stress the weld locked in.

Steel Sheet Flatness Tolerance Before Cutting and Bending

Read flatness by thickness, width and strength class, specify normal or special, and keep parts clear of the edge wave strip.

What a Flatness Tolerance Covers Before the First CutIn the EN 10131 and EN 10051 tables, as ArcelorMittal prints them, flatness is a maximum deviation in millimeters, and the tables apply to sheet, not to coil. The extract does not describe the set-up used to measure it.

Laser Cut Part Dimensional Tolerance Under ISO 9013 Class 1 and Class 2

Pick the tighter or looser dimensional class per feature, read inside and outside sizes at their extremes, and anchor fit features to each other.

What Dimensional Tolerance Class 1 and Class 2 Cover on a Laser Cut PartISO 9013:2017 applies to laser cuts from 0.5 mm to 32 mm in thickness. Its clause 8 gives limit deviations for nominal dimensions in two classes, listed in Table 6 for class 1 and Table 7 for class 2.

316L Stainless Steel Sheet for Laser Cutting and Bending

Choose the molybdenum-bearing low-carbon grade for chloride exposure, plan overbend on the brake, and write the finish and weld tint rules on the drawing.

What 316L Sheet Adds Over 304L in a Cut and Bent PartType 316L is Type 316 with the carbon ceiling lowered from 0.08 % to 0.03 % by weight. Both carry 16.0 to 18.0 % chromium, 10.0 to 14.0 % nickel and 2.00 to 3.00 % molybdenum, according to the Cleveland-Cliffs product bulletin for the two types.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote