Meaning
Lack of fusion is an ISO 5817 weld imperfection, never permitted at the surface and allowed in micro form only at levels D and C. A quality level controls it like the other listed imperfections. TWI’s welding advice also stops at the setting that would cause it.Surface Lack of Fusion
In material 0.5 mm (0.02 in) and thicker, ISO 5817 permits no surface lack of fusion at D, C or B. It shares that rule with cracks, crater cracks and burn through. A drawing that names any level therefore rejects it.Read More
Micro Lack of Fusion
The standard defines micro lack of fusion as detectable only at 50 times magnification or more. It is permitted at levels D and C, and not at B. Under macro-examination, only imperfections visible at up to ten times count, with micro lack of fusion excluded from that rule. Internal lack of fusion has its own row in the standard’s table of internal imperfections.Welding Practice
TWI’s distortion advice runs into this imperfection. To limit distortion, it favors the largest electrode diameter or highest current that does not cause lack of fusion. It also favors depositing weld metal quickly with the fewest runs. Sound fusion is therefore the ceiling on current and wire size in that advice.Inspection
ISO 5817 does not describe how to detect imperfections. Visual testing finds surface lack of fusion. Internal forms need the non-destructive methods ISO 17635 links to the levels, set out in the contract. The extent of that testing is set in the contract, beside the quality level.