Boiling Water Test

The boiling water test is the first half of the minimum adhesion check IGP's powder data sheet sets for coated aluminum and galvanized parts.

Every Boiling Water Test article of the Sheet Metal Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The boiling water test is the first half of the minimum adhesion check IGP’s powder data sheet sets for coated aluminum and galvanized parts. The coated part goes through the boiling water test first. A cross-cut adhesion and tape test follows. The pair confirms that the pretreatment holds the powder on these two substrates.

Why These Metals

IGP names aluminum and galvanized steel, not bare steel, for this minimum. Each has its own pretreatment list. Aluminum takes chromating, pre-anodizing or a chrome-free system, and galvanized steel takes phosphating, passivation or chromating. The minimum test therefore reads as a warning that these substrates hold coatings less forgivingly than bare steel.
Read More

Who Runs It

IGP leaves the choice of pretreatment to the coater, to be tested in advance. Its data sheet refers to the guidelines of GSB International, Qualicoat and Qualisteelcoat. The test belongs to the coater’s qualification of a pretreatment and powder on a given metal.

On the Order

A coating note on an aluminum or galvanized part names the powder system and the pretreatment standard. It also asks for the adhesion result on the first lot. The buyer then has the coater’s proof before the batch is released.

Not a Corrosion Test

The boiling water test checks adhesion after exposure, not corrosion life. IGP’s condensation water and salt spray results, 500 to 1,000 hours, are separate long tests. They belong to the powder system’s qualification, not to each lot. IGP also marks those hours as dependent on the pretreatment used.

Powder Coated Sheet Metal Batch From Pretreatment to Cure and Inspection

A powder coating cures in minutes but depends on pretreatment, rack mass and film allowance, and a lot is judged on gloss, film and adhesion, not corrosion hours.

The Stages a Coated Batch Passes ThroughA batch of sheet metal parts goes through six stages on its way from the bare part to a coated one: pretreatment, drying, masking and hanging, application, cure, and cooling and packing. Each stage has a condition the powder maker states, and each has its own place in the schedule.

Galvanized Steel Sheet Coating Weight Designations for Cut and Welded Parts

Read the coating designation as a minimum zinc mass over both faces, name the standard and test basis, and plan ventilation for cutting and welding.

What a Coating Weight Designation Says About the SheetA designation states the minimum mass of zinc, or zinc alloy, on the sheet and the units it is stated in. G90 means hot-dip galvanized, with a triple spot test average of at least 0.90 ounce per square foot, counted over both sides together.

5052 H32 Aluminum Sheet for Bending and Welding

Name the alloy, temper and specification, draw bend radii from a trial bend at the real thickness, and design welded joints to the annealed strength the weld leaves.

What 5052 H32 Offers a Bent and Welded Aluminum PartAlloy 5052 is an aluminum-magnesium alloy, registered in the United States in 1954. The Aluminum Association's international alloy register sets its composition: silicon 0.25 % maximum, iron 0.40 %, copper 0.10 %, manganese 0.10 %, magnesium 2.2 to 2.8 %, chromium 0.15 to 0.35 %, zinc 0.10 %, and 0.05 % each and 0.15 % in total for other elements, with aluminum the remainder.

Request a Sheet Metal Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Sheet Metal chosen.

Request a Quote